Sign In to gain access to subscriptions and/or personal tools.
|
Microcracks in Dental Porcelain and Their Behavior during Multiple Firing
J.R. Mackert, Jr
Section of Dental Materials, Department of Oral Rehabilitation, Medical College of Georgia, Augusta, Georgia 30912-1260, USA
A.L. Williams
Section of Dental Materials, Department of Oral Rehabilitation, Medical College of Georgia, Augusta, Georgia 30912-1260, USA
Dental porcelains rely on the high-thermal-expansion mineral leucite to elevate their bulk thermal expansion to levels compatible with dental PFM alloys. The microcracks that form around these leucite particles when cooled during porcelain manufacture are a potential source of change in bulk porcelain thermal expansion during fabrication of porcelain-fused-to-metal crowns and bridges. The purpose of the present study was to determine whether multiple firings of commercial dental porcelains could produce changes in microcrack density. Specimens of six commercial porcelains and the "Component No. 1" of the Weinstein patent were fabricated and subjected to 1, 2, 4, 8, and 16 firings. The microcrack densities were determined by quantitative stereology, whereby intersections of microcracks were counted with a test grid. The microcrack data were subjected to linear regression analysis and analysis of variance. The microcrack densities of four of the six porcelains and the Component No. 1 frit were not significantly affected by the number of firings (p > 0.05). One porcelain exhibited a weak but highly significant positive correlation between microcrack density and multiple firings ( r2 = 0.24, p = 0.0003), while the remaining porcelain exhibited a weak but statistically significant negative correlation between microcrack density and multiple firings (r2 = 0.15, p = 0.006). The results of this study indicate that even for porcelains that exhibit a measurable change in microcrack density as a function of multiple firings, the magnitude of the increase or decrease in microcrack density after several firings is sufficiently small to cause only negligible shifts in porcelain bulk thermal expansion.
Key Words: ceramics dental porcelain microcracking leucite, stereology
REFERENCES
- Binns D. (1983). The chemical and physical properties of dental porcelain, In: Dental ceramics, Proceedings of the first international symposium. McLean JW, editor. Chicago: Quintessence Publishing Co., Inc., pp. 41-82.
- Dorsch P. (1981). Stresses in metal-ceramic systems as a function of thermal history. Ceramic Forum Int/Ber Dt Keram Ges 58:1-7.
- Dorsch P. (1982). Thermal compatibility of materials for porcelain-fused-to-metal (PFM) restorations. Ceramic Forum Int/Ber Dt Keram Ges 59:1-5.
- Fairhurst CW, Anusavice KJ, Hashinger DT, Ringle RD, Twiggs SW (1980). Thermal of dental alloys and porcelains. J Biomed Mater Res 14:435-446.[Medline]
[Order article via Infotrieve]
- Hall FP ( 1930). The influence of chemical composition on the physical properties of glass. J Am Ceram Soc 13:182-199.
- Hoshikawa T., Agaki S. (1972). Formation of leucite and thermal expansion in SiO2-Al2O3-K2O-Na2O glasses. Yogyo-Kyokai-Shi 80:42-48.
- Kingery WD, Bowen HK, Uhlmann DR (1976), Introduction to ceramics, 2nd ed. New York: John Wiley & Sons, pp. 583-644.
- Mackert JR Jr (1988), Effects of thermally induced changes on porcelain-metal compatibility. In: Perspective in dental ceramics, Proceedings of the Fourth International Symposium on Ceramics, Preston, JD, editor. Chicago: Quintessence publishing Co., pp. 53-64.
- Mackert JR Jr, Evans AL (1991a). Effect of cooling rate on leucite volume fraction in dental porcelain. J Dent Res 70:137-139.
- Mackert JR Jr, Evans AL (1991b). Quantitative x-ray diffraction determination of leucite thermal instability in dental porcelain. J Am Ceram Soc 74:450-453.
- Mackert JR Jr, Rueggeberg FA, Lockwood PE, Evans AL, Thompson WO (1994). Isothermal anneal effect on microcrack density around leucite particles in dental porcelain. J Dent Res 73:1221-1227.
- Morey GW (1954). The properties of glass. New York: Reinhold, pp. 271-273.
- Nielsen JP, Tuccillo JJ (1972). Calculation of interfacial stress in dental porcelain bonded to gold alloy substrate. J Dent Res 51:1043-1047.
- Prasad A., Day GP, Tobey RG (1988). A new dimension for evaluation of porcelain-alloy compatibility. In: Perspectives in dental ceramics, Proceedings of the Fourth International Symposium on Ceramics. Preston JD, editor. Chicago: Quintessence Publ. Co., Inc., pp. 65-74.
- Underwood EE (1970). Quantitative stereology. Reading, MA: Addison-Wesley Publishing Co., pp. 38-40.
- Vergano PJ, Hill DC, Uhlmann DR (1967). Thermal expansion of feldspar glasses. J Am Ceram Soc 50:59-60.
- Weinstein M., Katz S., Weinstein AB, inventors (1962). Permadent Manufacturing Corporation, assignee. Fused Porcelain-to-Metal Teeth. US Patent 3,052,982. Sep 11.
- Yamamoto M. (1985). Metal-ceramics. Chicago: Quintessence Publishing Co., pp. 156-202.
Journal of Dental Research, Vol. 75, No. 7,
1484-1490 (1996)
DOI: 10.1177/00220345960750070801

CiteULike Complore Connotea Del.icio.us Digg Reddit Technorati Twitter What's this?
|
|