Advanced Search

Journal Navigation

Journal Home

Subscriptions

Archive

Contact Us

Table of Contents

CiteULike is a free service for managing and discovering scholarly references - click here to get started.

Sign In to gain access to subscriptions and/or personal tools.
Journal of Dental Research
This Article
Right arrow Full Text
Right arrow Full Text (PDF)
Right arrow Alert me when this article is cited
Right arrow Alert me if a correction is posted
Services
Right arrow Email this article to a friend
Right arrow Similar articles in this journal
Right arrow Similar articles in PubMed
Right arrow Alert me to new issues of the journal
Right arrow Add to Saved Citations
Right arrow Download to citation manager
Right arrowRequest Permissions
Right arrow Request Reprints
Right arrow Add to My Marked Citations
Citing Articles
Right arrow Citing Articles via Google Scholar
Right arrow Citing Articles via Scopus
Google Scholar
Right arrow Articles by Sano, H.
Right arrow Search for Related Content
PubMed
Right arrow PubMed Citation
Right arrow Articles by Sano, H.
Social Bookmarking
 Add to CiteULike   Add to Complore   Add to Connotea   Add to Del.icio.us   Add to Digg   Add to Reddit   Add to Technorati   Add to Twitter  
What's this?

Microtensile Testing, Nanoleakage, and Biodegradation of Resin-Dentin Bonds

H. Sano

Department of Restorative Dentistry, Division of Oral Health Science, Hokkaido University Graduate School of Dental Medicine, North 13, West 7, Kita-ku, Sapporo 060-8586 Japan; sano{at}den.hokudai.ac.jp


Figure 1
View larger version (66K):
[in this window]
[in a new window]

 
Figure 1. Microtensile testing and nanoleakage. (A) Original microtensile bond-testing. Resin-bonded specimens were cut perpendicular to the adhesive structure (left). Specimens were trimmed and shaped to a gentle curve along the adhesive interface. They were then attached to the testing device and tested in tension (right). C: cured resin composite. D: dentin. (B) Nanoloeakage expression at the adhesive interface. The hybrid layer showed extensive silver uptake, shown here as a white image because of its high atomic number. Slight silver staining was also observed within the cured adhesive layer.

 

Figure 2
View larger version (66K):
[in this window]
[in a new window]

 
Figure 2. Water-tree formation and pathway of biodegradation. (A) Different types of nanoleakage expression at the resin-dentin interface. Water-treeing was observed within the adhesive resin (arrow) (courtesy of Dr. F.R. Tay). (B) Pathway of degradation. (1) The first stage of biodegradation involves acid-etching to remove the smear layer and expose the fibrillar matrix. Then resin infiltration into the fibrillar matrix occurs. (2) The second stage involves hydrolysis and extraction of resinous materials within the hybrid layer, exposing collagen fibrils. (3) The third stage involves enzymatic attack by matrix metalloproteinases (MMPs), leading to slowly hydrolyzing collagen fibrils in the hybrid layer. Finally, depletion of collagen fibrils within the hybrid layer takes place, leading to loss of hybrid layer, loss of dentin seal, and loss of retention. (4) There is no evidence of remineralization of the adhesive interface following the use of dentin bonding systems in vivo, although that would be a desirable outcome.

 

Journal of Dental Research, Vol. 85, No. 1, 11-14 (2006)